Insulation Paper DDP Diamond Dotted Paper (kraft paper)

Insulation Paper DDP Diamond Dotted Paper (kraft paper)

Product DescriptionBrief IntroductionDiamond Dotted Insulation Paper( DDP) is made of electrical insulation paper with Diamond-shape epoxy resin dotted in both sides. The epoxy resin used in DDP contains a kind of incubative hardener material, it is a…

Product Description

Brief Introduction
Diamond Dotted Insulation Paper
( DDP) is made of electrical insulation paper with Diamond-shape epoxy resin dotted in both sides. The epoxy resin used in DDP contains a kind of incubative hardener material, it is a dry ad crisp material at normal temperature(below 35degree)

This product has good dielectric properties and good machenical properties after being heat-solidification. It can be used as coils and between layers of oil immerged power and distribution transformers.

Thickness; 0.08mm 0.13 0.15 0.17 0.20 0.25 0.38mm
Made of kraft paper coated with heat curable epoxy resin, the epoxy adhesive is applied to both sides of the paper in a diamond pattern consisting of 9.5mm X 9.5mm diamonds with 15.9mm center spacing
Insulation Paper DDP Diamond Dotted Paper (kraft paper)
Insulation Paper DDP Diamond Dotted Paper (kraft paper)
The Diamond Dotted Paper, alias such as: Epoxy adhesive diamond paper, Diamond Dotted Presspaper, Double sided Diamond Pattern Paper, DDPP, DPRCP, D. D. P, DPP, Diamond Dotted insulating Paper, Varnished Paper, etc.

It is to be used in oil-immersed transformers for the insulation between of coils. On the insulation layer, there is a layer dotted epoxy resin that will be changed with high temperature change that is to be called as felt...

It is a kind of material with inertia, dry and no conglutination at normal temperature (below 30 degree C). The Diamond Dotted paper will make the electric conductor forever felt up as a hard unit under the high temperature by its internal latency substance. When the temperature is rising up to 90 degree C, The diamond dotted paper begins one-off thaw and then one-off solidification. When to keep the temperature at 90 degree C for 90 minutes, the epoxy resin would paste on neighboring cable and paper safely. The felt intensity is as high as to 70psl at 100 degree C (The value at least is equal to 0.275Mpa, America standard)
 
Typical properties of Diamond Dotted Paper
Specified PropertiesUnitsStandard
Thickness Toleranceinch0.0030.0500.0700.0100.0150.020
Mm0.0760.1300.1800.2500.3800.500
Thickness tolerance(base paper)%±10
Width tolerancemm± 5
Apparent Densityg/mm^30.95 - 1.15
Tensile strength Min  Machine directionN/mm2707080808080
corss machine direction353535353535
Elongation MD%2
CD4
Dielectric breakdown (volts/layer, dry test)volts75011001400210029003100

No pollution oil of transformer%Non pollution
Moisture Content%4.0-8.0,all thickness
PH water extract%6.0-8.0, all thickness
Ash Content Max%1% maximum
Bond Strength MinkPa450
Coating thickness per sidemm0.006 to 0.012
All date shown represents nominal o typical vlues only and should not be construed or maximun unless specifically stated